Brand Name: | XUANLI |
---|---|
State: | Powder Coating |
Application Method: | Spray |
Usage: | metal surface coating |
Main Raw Material: | Epoxy |
Place of Origin: | China (Mainland) |
MF: | Xuanli |
RAL Cards: | 213 kinds of colors |
PANTONE Cards: | 1690 kinds of colors |
Quick Details
Specifications
(1) Spray ratio is 90%;
(2) 1KG of powder coating can spray 8-10 square meter;
(3) Powder Coating adhesive force is stronger 8-10 years;
(4) Powder Coating is not easy to fade in 5-8 years;
2. Charactcristic: Powder
Available Powder Types | Available Colors |
1. Epoxy powder coating | 1. RAL Colors |
2. Polyester Powder Coating | 2.Pantone Colors |
3.Epoxy-Polyester Powder Coating( Hybrid) | 3.Customer color matching |
4.Polyurethane Powder Coating | Available finish |
5.Heat transfer printing powder coating | 1. Smooth |
Available gloss level | 2. Rough( Sand texture ) |
1. High gloss( Above 80%) | 3.Wrinkle( fine texture ) |
2. Flat gloss (50%-80%) | 4.Antique( hammer tone) |
3. Semi gloss(5%-50%) | 5.Metallic |
4. Matt ( below 5%) | 6.Other special effect ( artistic) |
Bad symtoms | Possible Cause | Solution |
1.With low power, powder coating is not easy to coated;
|
1. High voltage power supply shortage; | 1.Check the circuit |
2.Grouding is bad; | 2.Remove clutter grouding line | |
3.Compressed air volume is too big, the powder to blow fell &blows away; |
3.Spray appropriate isolation, reduct air convection; |
|
4.Powder particle size is too thin; |
4.Add new powder coating, reduce the recovery powder consumption. |
|
5.The air temperature is too high; |
5.Powder particles with air water branch of low power, control temperature of spray area; |
|
2. Charge repulsion powder repboud from the working surface; |
1.The voltage is too high; | 1. Lower voltage and air volume; |
2.Spray gun from the work location is too close; |
2. Extend the spray gun and artifacts; | |
3. Grouding is bad; | 3.Remove clutter grouding line; | |
4.Powder particle size is too thin, not esay to attach to the workpiece surface; |
4.Add new powder coating, reduce the recovery powder consumption; |
|
3. Corner not easy spraying penetration is bad; |
1. The powder amount is too small; |
1. Lower voltage and air volume, increasing the amount of powder; |
2. Grouding is bad; | 2. Adjust the spray gun position; | |
3. The voltage is too high; | 3. Choose small backboard, proper nozzle; | |
4. Spray gun position is not good; |
4.If the corner is more and deeper, then consider friction gun equipment; |
|
5. Powder spraying range is too wide; | ||
4.Powder spraying uneven | 1. Air pressure is insufficient; | 1. Cleaning pipeline, spray gun and flowmeter; |
2.Line fault block; |
2.Check the air supply, Exclude water vapor in powder agglomeration; |
|
3.Block in the spray gun; |
3.If powder agglomeration, to screen or change new powder coating; |
1.1KG of powder coating can spray 8-10 square meter;
2.Spray ratio is 95 %;
3.Powder coating adhesive force is stronger 8-10 years;
4.Powder coating is not easy to fade in 5-8 years;
Card Types | Color Category |
1. RAL Cards | 213 kinds of colors |
2. PANTONE Cards | 1690 kinds of colors |
3. FRD Cards | 360 kinds of colors |
Our service
1. We offer professional products and fast delivery.
2. We will help you solve problems when you use our products.
3. Any question can turn to the technology department of our company.
Our Product specially designed for surface decoration product such as home furniture, electrostatic appliance, industrial equipment, sports equipment, harware, shop tool rack, lamps and lanterns, computer chassics, DVD sheel, etc.
Application Area | |
1. Household Applications | 7. Used for Security Door; |
2. Car Coating | 8. Radiator & Heat Sink; |
3. Used for Valve | 9. Corrosion Prevention of Pipes; |
4. Track Traffic | 10. Communications Equipments; |
5. Aerospare field | 11. Hardware & Brightwork; |
6. Fitness Equipment | 12. Zincing & Aluminium; |
Application Parameter:
Item |
Standards |
Properties |
Results |
Pencil hardness |
GB/T 6739 |
≥ H |
To agree panel |
Impact resistance |
GB/T 1732 |
≥ 50 kg |
To agree panel |
Flexing endurance |
GB/T 6742 |
≤ 2mm |
To agree panel |
Adhesive force |
GB/T 9286 |
Grade 0 |
To agree panel |
Bend test |
GB/T 6742 |
2mm |
To agree panel |
Color difference |
GB/T 9761-1988 |
No obvious color difference |
To agree panel |
Heat text |
|
500h |
>500h |
Remark |
1. The above test use cold-rolled steel (thickness: 0.8mm) to remove rust and oil. Suggested film thickness: 60—80 um 2. All the indicators of film features will be down lightly depending on reducing of luster. |