SPECIFICATION & PARAMETER
MATERIAL
Surface layer: BOPP
glue layer: EVA adhesive
SPECIFICATION
Thickness: GLOSSY: 25μm(12+13) 27μm(15+12) 30μm(18+12)
MATTE: 27μm(15+12) 30μm(18+12)
Width: 310~1880mm
Length: 100~3000M
Paper core: 25.4mm (1 inch),58mm(2.25inches),76mm(3 inches)
BONDING: less than 2
Process Parameter:
Equipment for thermal film: dry and wet film laminator
lamination temperature: 95~105℃
Roller pressure: 10-20Mpa
Speed: 8-20 m/min
Directions for using BOPP thermal laminating film:
Normal process temperature is 90℃-105℃, roller pressure and temperature vary with different types of paper, ink and machines.
When using the film for the first time or do other treatment, try a small volume before mass laminating.
Make sure the ink is dry before laminating. It will delaminate when the paper contains too much moisture and powder.
Make sure put the material in a low-temperature, dry place.
Characteristic:good plasticity and smoothness, low density,good transparency, strong chemical resistance, suitable for low temperature lamination, stable printing ink color after laminating. BOPP thermal glossy film is high transparency and clarity, color enhancement; BOPP thermal matte film can extinction and keep the color from change.
PRODUCT APPLICATION
publications cover
Eg: Magazines, Books, Paper bags, Maps, and publicity materials
Package
Eg: Wine, Food, Medicine, daily consumer goods
Advertisement
Eg: Advertisement paper, Board, Drawing, Document, and Photos