Ingredient |
Nickel |
Copper |
Manganese | ||
Content |
39-41 |
Remainder |
1-2 | ||
Skin material specification |
Thick |
≥0. 1mm | |||
Width |
According to customer demand formulation | ||||
Silk material specification |
≥0. 1mm | ||||
Average resistance temperature coefficient |
4040×106C1 | ||||
Tensile strength |
≥390Mpa | ||||
Elongation ratio |
≥12 | ||||
To copper thermo-electromotive force |
-45uV/ | ||||
Electronic resistivity |
0. 48±0. 03uΩ. M | ||||
Characteristic and use |
It is the electric resistance alloy with the copper nickel as the essential component. It has the low resistance temperature coefficient, wide working temperature scope (500 below), good machining property, anti-corrosive and easy braze welding. Used in manufacturing regenerator's variable resistor and the strain resistor. |