Refractory liner casting construction of industrial furnace that needs quick production resuming with short construction period;
Casting construction of extra thick furnace liner and hard drying position (e.g. furnace hearth);
Local repair of refractory liner and quick drying.
Model |
LM-D55 |
LM-D65 |
LM-D70 | |
Al2O3% |
≥55 |
≥65 |
≥70 | |
MPa
Crushing strength |
110℃×24h |
≥25 |
≥20 |
≥25 |
1400℃×3h |
≥50 |
≥40 |
≥60 | |
Hardening time |
12~24h |
12~24h |
12~24h | |
Heating up time to 650℃ |
48~72h |
48~72h |
48~72h | |
℃
Maximum service temperature |
1450 |
1500 |
1550 | |
℃
Refractoriness |
1700 |
1750 |
1790 | |
g/cm
Bulk density |
2.30 |
2.35 |
2.40 |