Perforated ceramic ball is developed on the basis of inert ceramic ball. It has an adequate mechanical strength, chemical and thermal stability as the normal inert one; furthermore, it has higher dispersion and flux of the fluids, more surface area and lower resistance results from the perforated holes on the ball body. As a new efficient support and covering material of catalyst, it has been widely used in oil refinery, chemical, fertilizer, natural gas and environmental protection industries since put into market.
Main specification:
Features | Feldstar | feldstar-mulite | mulite | mullite-corundum | corundum | |
Chemical compositon | Al2O3 | 20-30 | 30-45 | 45-70 | 70-90 | ≥90 |
Al2O3+SiO2 | ≥90 | |||||
Fe2O3 | ≤1 | |||||
Water absorption % | ≤5 | |||||
Acid resistance % | ≥98 | |||||
Alkali resistance % | ≥80 | ≥82 | ≥85 | ≥90 | ≥95 | |
Refractory temperature ℃ | ≥1300 | ≥1400 | ≥1500 | ≥1600 | ≥1700 | |
Crushing Strength N/Particle | φ6 | ≥400 | ≥420 | ≥440 | ≥480 | ≥500 |
φ8 | ≥480 | ≥520 | ≥600 | ≥620 | ≥650 | |
φ10 | ≥600 | ≥700 | ≥800 | ≥900 | ≥1000 | |
φ13 | ≥1000 | ≥1100 | ≥1300 | ≥1500 | ≥1800 | |
φ16 | ≥1500 | ≥1600 | ≥1800 | ≥2300 | ≥2600 | |
φ20 | ≥1800 | ≥ | ≥2300 | ≥2800 | ≥3200 | |
φ25 | ≥2500 | ≥2800 | ≥3200 | ≥3600 | ≥4000 | |
φ30 | ≥3000 | ≥3200 | ≥2500 | ≥4000 | ≥4500 | |
φ38 | ≥4000 | ≥4500 | ≥5000 | ≥5500 | ≥6000 | |
φ50 | ≥6000 | ≥6500 | ≥7000 | ≥8500 | ≥10000 | |
φ60 | ≥8000 | ≥8500 | ≥9000 | ≥10000 | ≥12000 | |
φ75 | ≥10000 | ≥11000 | ≥12000 | ≥14000 | ≥15000 | |
Bulk Density Kg/m3 | 1100-1200 | 1200-1300 | 1300-1400 | 1400-1500 | ≥1550 | |
Remark: The data of bulk density is only as referecne, not as inspection basis. |