Product Main

Specifications

2000production description(super poly putty)
Application & characteristic:
 
The optimal comprehensive function, excellent apply property, particularly easy burnishing, and there is no pinhole as well as sand hole, improvement of efficiency. Especially suitable for 4S firm, various precision instrument and advanced automotive whole –painting.
 
Scope of construction: It can be used in iron panel, steel plate, aluminium plate and on any painted metallic surface.
 
 
Main performance indexes:  
 
Item
indexes
    Test method
Flexibility(mm)
50
GB/T1748
Impact strength(kg.cm)
≥25
GB/T1732
Thermal resistance
(1h baking under
140℃)
No bubble, no crack
GB/T1735
Adhesion
First class
Bending method
Temperature variation resistance
(3cycles)
No bubble, no crack
Eye test 
Sanding property
Easy sanding, extraction powder is fast
Hand feel
 
 
 
 
 
 
 
 
 
 
 
 
 
P.S: Temperature variation resistance -40℃1h—1h(at ambient temperature)—120℃1h is a cycle.
 
Application:
1.Remove the oil, rust, original paint film and water etc. from surface completely, keep the painted surface clean & dry before scraping.
2.The putty may cause uneven in the process of storage, must use clean ruler stir well before using.
3,The putty and hardener should be mixed completely to achieve the uniformity of color (general ratio is 100:2 by weight), and apply the mixture within potlife(3-8min), or it will gel.
4,Apply the mixtured putty to the processed surface of primer or cold-reduced sheet, in case of scraping of thick coat, it is preferable to apply in thin coats for several times till reaching the objective thickness.
(Suggested maximum thickness is no more than 5mm).
5,Wet milling or dry milling should be made after hardened thoroughly. The best wet milling time is 0.5-1h after applying putty, best dry milling time is about 2h after applying putty(The temperature is 25℃, humidity is less than 40%). Ensure the putty has been completely dry when painting, lest drop off or bubbles.
 
Notices:
1,When there is air bubble while applying, fully scrape to evenness with spatula to ensure good adhesion.
2,The putty mixed with hardeners should not be returned to the original container, container which is opened must be carefully resealed, lest volatilization &d eterioration of solvent. Do not mix lacquer thinner to putty.
3 ,When there is low temperature or high relative humidity, curing time of coating will be extended somewhat. The corresponding adjustment can be made to the consistency and gel time of putty according to per customer's request.
4,Our product matches with various primers, but not in phenolic primers and alkyd primers, lest drop off or bubbles. Ensure the primer has been thoroughly dry when applying putty, or cause drop off.
5,The product should not apply in galvanized sheet directly.
6,The shelf life can be up to 12 months at the cool place (under 25℃).