low carbon as steel back with copper alloy powder sintered on the surface.
Thickness of the steel back |
0.6-5.0mm |
Max applicable temperature |
260oC |
Thickness of alloy |
0.2-2.0mm |
Friction coefficient |
≤0.12 |
Alloy material |
CuPb10Sn10 |
Alloy hardness |
60-90HB |