High Alumina Cement
|
The index of Alumina cement | |||||||
|
Aluminate cement |
CA40-Fused |
CA50-J5 |
CA50-J6 |
CA50-J7 |
CA50-N |
CA50-J9 |
CA50-Fused |
|
Blaine (cm2/g) |
≥2700 |
≥3000 |
≥3000 |
≥3000 |
≥3000 |
≥4000 |
≥4000 |
|
Initial time(h:m) |
≥0:40 |
≥0:30 |
≥0:30 |
≥0:30 |
≥0:30 |
≥1:30 |
≥2:00 |
|
Final time(h:m) |
≤4:00 |
≤6:00 |
≤6:00 |
≤6:00 |
≤6:00 |
≤6:00 |
≤6:00 |
|
Flexural strength(Mpa) |
6hrs≥4.0 |
|
|
|
|
|
≥4.0 |
|
1 day |
≥5.5 |
≥5.5 |
≥6.0 |
≥6.5 |
≥6.0 |
≥8.0 |
≥10.0 |
|
3 days |
≥6.5 |
≥6.5 |
≥7.0 |
≥7.5 |
≥7.0 |
≥10.0 |
≥11.0 |
|
Compressive strength |
6hrs≥30.0 |
|
|
|
|
|
≥35.0 |
|
1 day |
≥50.0 |
≥40.0 |
≥45.0 |
≥50.0 |
≥50.0 |
≥70.0 |
≥75.0 |
|
3 days |
≥60.0 |
≥50.0 |
≥55.0 |
≥60.0 |
≥60.0 |
≥80.0 |
≥85.0 |
|
Chemical composition |
|
|
|
|
|
|
|
|
SiO2 % |
≤6.0 |
≤8.0 |
≤8.0 |
≤8.0 |
≤6.5 |
≤6.0 |
≤5.0 |
|
Al2O3 % |
≥37.0 |
≥50.0 |
≥50.0 |
≥51.0 |
≥50.0 |
≥53.0 |
≥50.0 |
|
CaO % |
≤38.0 |
≥33.0 |
≥33.0 |
≥33.0 |
≥33.0 |
≥33.5 |
≤38.0 |
|
MgO % |
≤1.5 |
≤1.5 |
≤1.5 |
≤1.5 |
≤1.5 |
≤1.5 |
≤1.5 |
|
TiO2 % |
≤3.0 |
≤3.0 |
≤3.0 |
≤3.0 |
≤3.0 |
≤3.0 |
≤3.0 |
|
Fe2O3 % |
≤18.0 |
≤3.0 |
≤3.0 |
≤2.5 |
≤3.0 |
≤2.5 |
≥50.0 |