Index |
Specificatiom | ||
Appearance |
Brown Sphere | ||
Sphere Size mm |
Φ 1--2 |
Φ 2--4 |
Φ 3--5 |
Bulk Density g/cm3 |
0.68--0.74 |
0.64--0.70 |
0.60--0.68 |
Crush Resistance N/sphere |
≥14 |
≥40 |
≥60 |
Abrasion Loss WT% |
≤0.30 | ||
Static Absorbing Capacity RH60% |
≥20 |
Molecular sieve 3A is mainly used for deeper-drying in oil gas, ethylene, propylene and petroleum natural gas.