Firebricks for steel ladle
ITEM |
Firebricks for Steel Ladle | |
INDEX |
CN-40 |
CN-42 |
Al2O3 %≥ |
40 |
42 |
Refractoriness,℃≥ |
1730 |
1750 |
0.2MPa refractoriness under load,℃≥ |
1400 |
1430 |
Linear change after heating,%1400℃ 2h |
0
-0.3 |
0
-0.3 |
Apparent Porosity,%≤ |
19 |
18 |
Cold Crushing Strength,MPa≤ |
34.3 |
39.2 |