The products are widely used in the production of rubber tires and solid tires, it has the good features to improve the plasticing, and it is helpful to decrease the cost.
Tensile strength
|
Elongation percentage
|
Mooney viscosity
|
Ash content
|
≥MPA
|
≥%
|
ML100℃@1+4
|
≤%
|
4.0MPA
|
220%
|
50-65
|
16
|
5.0MPA
|
250%
|
50-65
|
15
|
6.0MPA
|
260%
|
50-65
|
15
|
7.0MPA
|
280%
|
50-65
|
15
|
8.0MPA
|
290%
|
50-70
|
13
|
9.0MPA
|
310%
|
55-70
|
12
|
10.0MPA
|
350%
|
65-75
|
11
|
11.0MPA
|
370%
|
65-75
|
10
|
12.0MPA
|
390%
|
70-85
|
8
|