Product Main

Specifications

 
Features:
The product is processing with precise configuration by high quality cement, ultra-fine hard aggregate and various organic polymer additives. High Viscosity \ Good flowability  \ Well Adhesion. And can be used in many grounds cushion of basic layer.
Application:
It can be used in leveling of bases to be covered with wood floor\ carpet \ PVC rubber floor. And used in leveling with requirements or epoxy-coated needs of base\ other grounds with dust-proof needs. Such as: residential building \ hospital \ shopping malls.
 
Specification: Standard: JC/T985-2005
Items    
Test data                                   
Index
flowability (mm)
Initial flowability
270
≥130
20min flowability
200
≥130
Tensile adhesive strength(M pa)
1.1
≥1.0
Dimensional change rate,%
-0.04
-0.15~+0.15
24h compressive strength(M pa)
6.1
≥6.0
24h bending strength(M pa)
2.0
≥2.0
28h compressive strength(M pa)
43.4
≥40
28days anti-bending strength(M pa)
5.7
≥4
How to use
1 Surface preparation:
1st First the strength of the concrete surface, before working should ≥C20, and make sure no lose part \ sand  \dust \ oil on the surface . Keep surface hard, smooth and clean.
2nd Spray water on the concrete surface, make sure moist enough before construction. Make sure clean and no water on the surface during construct.
3rd The new base of general Portland cement should do self-leveling construction after 21days, and after 7days for sulphoaluminate cement.
2 Mixing:
1st As for small area and road construction, you can stir with a small electric mixer in the bucket. As for large area construction, stir with high-speed mixer and use mortar pump to construct.
2nd Mix 5-6kg water with HGM-80 Self-leveling Mortar one bag (20kg), stir 4-5 min, after place for 1 min, stir again to even. Construction in low temperature , it suitable to mix with 40℃ \104℉ water. 
3rd The construction temperature  ≥ 5℃\41℉,the mixed Self-leveling mortar should be used up within 35min.
3 Construction:
1st Make the mixed self-leveling mortar spread evenly , then control the thickness with special notched scraper .the construction thickness  ≥3mm is preferred, construction thickness with one time is 3~30mm, and the dosage is 1.6kg/m²/mm
2nd The operator can enter the construction ground with spike shoes, and screed with special notched scraper in order to eliminate uneven at the conjunction and maintain the required thickness.
4th Use the deflated cylinder to eliminate the bubble produced by mixing.
4 Curing:
Maintain like normal mortar under normal condition, spray water or cover with mat etc to curing 1—3 days.
 
Package & Storage
20kg±0.5 kg /bag ,12 months from manufacture date stored in dry \ cool place \ waterproof \ moisture proof with original package un-opened.