Used in paper making industry to wash and concentratethe pulp of low consistency.It can also be used for the recovery of fibers from white water.
Main Specifications:
1. Pulp inlet consistency:
0.35--0.45% (white water recycle);
0.5--1% (thicking for straw pulp or deinking pulp);
0.5--1% (OCC,wood pulp)
2.Pulp outlet consistency:
3.5--4.5% (white water recycle);
4--10% (thicking for straw pulp or deinking pulp.Adjustable)
4--12% (OCC,wood pulp.Adjustable)
3.Capacity:
2--2.6m3/m2h (white water recycle);
0.5--0.7t/d*m2 (thicking for straw pulp or deinking pulp.Adjustable)
0.7--1.1t/d*m 2(OCC,wood pulp.Adjustable)