Product Main

Specifications

 
 
            Name
                  
                      Chemical Composition (%)
 
C
 
  Si
 
Mn
 
    Cr
 
   P
 
   S
Mo,Al,Cu,Ni,Nb,Ti,Zr,V,B,Mg
 
High Chrome Alloyed Casting Ball
 
1.8-3.2
 
0.3-1.2
 
0.3-1.0
 
10.0-10.5
 
≤0.1
 
≤0.1
 
      Trace
 
Low Chrome Alloyed Casting Ball
 
2.0-3.5
 
≤1.2
 
≤1.0
 
0.5-1.5
 
≤0.15
 
 ≤0.25
 
      Trace
 
High Chrome Alloyed Casting Micro-Ball
 
1.8-3.3
 
0.3-1.2
 
0.3-1.0
 
10.0-10.5
 
≤0.1
 
≤0.1
 
      Trace
 
Low Chrome Alloyed Casting Micro-Ball
 
2.0-3.3
 
≤1.2
 
≤1.0
 
 0.5-1.0
 
≤0.25
 
 ≤0.15
 
      Trace
 
2. Machanical  Properties
 
 
 
           Name
 
 
                                                                              
   Machanical  Properties 
Specification
Surface Hardness
 
AK
(J/cm)
Microstructure
Times of Falling Balls
 
High Chrome Alloyed Casting Ball
 
Φ30-Φ130
 
  58-66
 
≥2.5
 
    M + C
 
    ≥10000
 
Low Chrome Alloyed Casting Ball
 
Φ30-Φ130
 
  ≥45
 
≥1.6
 
    P + C
 
    ≥8000
 
High Chrome Alloyed Casting Micro-Ball
 
Φ8-Φ25
 
  58-66
 
≥2.5
 
    M + C
 
    ≥10000
 
Low Chrome Alloyed Casting Micro-Ball
 
Φ8-Φ25
 
  ≥45
 
≥1.6
 
    P + C
 
    ≥10000
 
3. Heat Treatment
The domestic first MCGS uniform temerature graduation oil-quenched production line,uses the computer long-distance visualization control.The temperature and the oil temperature carry on the accuracy control to the stove. Guarantee quenching quality maximum limit.Hardness of product high chromium cast grinding ball is bigger than HRC 62.The difference of surface hardness and centre hardness is less than 2 HRC. Residual Austenite less than or equal to 5%, Martensite organization of thin strip.Application of ball consumption of less than or equal to 20g/ton.
4. Medium Frequency Induction Furnace
The medium frequency induction furnace we applied was developed by the Xi'an Jiaotong University, using 660V low-voltage power transmission, by improving the frequency power supply and control voltage current value , the maximum extent has accelerated the melting speed. Improve efficiency, reduce the burning of alloy elements, ensure the stability of the material.
5. Laboratory
We have a wear-resistant materials, provincial qualified R & D Center,  with the most advanced spark –direct reading spectrometer in the country, ultrasonic flaw detector, metallography microscope, universal material testing machine, drop ball testing machine and other testing equipment the maximum guarantee product quality and new product development.