one component Thermal curing adhesive
Features:
1. On the metal cover has a strong adhesive force
2. Good resistance to water and oil. Anti-aging properties
3. With wide technological adaptability, it can be adapted to drying channels and ovens. It is also suitable for bonding and solidification of two ends together to improve production efficiency.
4. Machine injection and manual injection are both available.
5. It has long storage time without deterioration, sediment or agglomeration.
Applications:
It is suitable for bonding of paper elements of filters and metal end caps of combustion motors.(air filter, fuel filter, oil filter)
1. Appearance: viscous liquid(color based on the need to configure ,color can be change according to customer requirements)
2. Density: 1.5 plus or minus 0.2 g/ml
3. Viscosity: 3.000-50.000 map.s
4. Nonvolatile content: greater than or equal to 98%
5. Curing conditions: 160℃--180℃ 12-20min
6. shear strength:(steel-steel)State at room temperature use greater than or equal to10kg/cm2
7. tensile strength: put the five fold filter paper which is high-29.5mm fold width-22mm insert the adhesive with 2.5mm thick, the curing filter paper--- Pull away from the strength between the metal use greater than or equal to 200N can damage
8. oil resistance and aging resistance.(135℃×192h)not degumming
9. Validity period: within 6 month from the date of production
10. Package: as your request
11. Attentions :
A. Should be stored in the shade.
B. Heat curing time and filter size, layer thickness and bake temperature, the heat transfer are related.
C. Viscosity can be adjusted according to user requirements.
instructions:
1. The surface of end cover should removed oil ,rust and other impurities, The adhesive should be smeared evenly on every corner of cap surface, Thickness is not less than 2mm.
2. With different equipment and conditions, the instrument will display temperature which is different from actual temperature around the filter. So you should undertake technology detection to assure temperature and ensure the best bonding. If the temperature is too low, bonding effect will be affected