Product introduction
|
Main Technical Specification
Raw Material
|
Polypropylene
|
Crack Elongation (%)
|
20 ±5
|
Type
|
Monofilament
|
Density (% g/cm3)
|
0.91±0.01
|
Fiber Dia (mm)
|
0.03±0.005
|
Melting Point (℃)
|
160---170
|
Tensile Strength (MPa)
|
≥450
|
Resistance to Acid,Alkali
|
Strong
|
Length (mm)
|
6,9,10,12,19
|
Water Absorbency
|
No
|
Application
1) Take place of asbestos and manufacture the asbestos cement products.
2) Make the light wallboard, insulation board and other building material.
3) Make the component of the concrete, tubing and board.
4) The sprayed concrete, such as tunnel,mine,culvert and side slope.
Package
1) Take place of asbestos and manufacture the asbestos cement products.
2) Make the light wallboard, insulation board and other building material.
3) Make the component of the concrete, tubing and board.
4) The sprayed concrete, such as tunnel,mine,culvert and side slope.
Package
Base on requirement of customer, carton and PP bag are available. 0.9kg/bag
Please Note:
1) Recommend Adding Amount:
Common 0.9kg/m³
2) Length:
6mm for mortar
12mm or 19mm for concret