Grade
|
Functional Values
|
Performance & Applications
|
|||
|
Density
g/cm3 |
Hardness
HRA |
Bending Strength N/mm2
|
|||
| TYG4C | 14.5-15.2 | >=89.5 | >=1420 | High strength and impact resistance, used in drilling on mining layers. | |
| TYG8 | 14.5-14.9 | >=89 | >=1570 | High strength and high shock resistance when use. Used for stones, blocks and in mining layers f = 8. | |
|
TYG8C
|
14.5-14.9 | >=88 | >=1720 | Good toughness and high strength. It is capable of resisting to high impact loads. Used for very hard stone and in mining layers f = 14. | |
| TYG11C | 14.0-14.4 | >=86.5 | >=2060 | Good thermal strength, high resistance for wearing and impacting. Used in drilling on very hard walls and cements. | |
| TYG15 | 13.9-14.2 | >=86.5 | >=2060 | High hardness and toughness. Used for very hard mining layers. | |
| TYG15C | 13.8 | >=86 | >=2450 | Optimum wearing resistance and high bending strength. Used for very hard mining layers. | |