CMC-Magic1
Very not easy to crack, suitable for high carbon content heat-treated steel.
Be used for embossing & drawing die, which can greatly reduce the scratches
caused by bending and stretching between high tension steel and ordinary one.
caused by bending and stretching between high tension steel and ordinary one.
CMC Tig Rod For Hard Surfacing
CMC-SKD11-3
Repair cold working steel (punch die)
Mending cut dies & shears
(Excellent welding usability, preheat is not required & no cracks
Hardness: HRC 56~58 No copper plating but great antirust property)
For welding cold work steels, punch dies, cutting dies & shears, piercing form, industrial knives, forming dies, harden surface of work piece.
This is a sort of high hardness, grinding-resisted, great toughness Argon filler rod.
CMC-SKD61-2
Repair hot working steel (forging die),Mending hot working form shears
(Excellent welding usability, preheat is not required & no cracks
High temperature resistant High hardness: HRC 52~57)
For welding hot forging die, hot cut die, hot punch die, hot formation die, hot work tool, steel casting die.
CMC-SKD61
Repair hot working steel (casting die)
Repair die casting die
(Design for Aluminum (Al) & Magnesium (Mg) die casting die
Hardness: HRC 42~46, Good machining property
High temperature resistant)
For welding Aluminum & Magnesium casting die. Extrusion dies.
Well heat-resisted, grinding-resisted, crack-resisted.
CMC-2365
Repair hammer forging dies
Repair hot working steel
(Design for hammer-forging die Hardness: HRC 42~46, Good machining property High temperature resistant)
For welding hammer-forging die, Aluminum & Copper hot forging die, Aluminum & Copper casting die.
great heat-resisted, grinding-resisted, crack-resisted.
CMC-8407-H12
Repair hot working steel (forging die)
Mending hot working form shears
(Excellent welding usability, preheat is not required & no crack
High temperature resistant High hardness: HRC 52~57)
For welding hot forging die, hot cutting die, hot punch die, hot formation die, hot work tool, steel casting die.
CMC-8407
Repair hot working steel (casting die)
Repair die casting die
(Design for Aluminum (Al) & Magnesium(Mg) die casting die
Hardness: HRC 40~45, Good machining property
High temperature resistant)
For welding the die made of the alloy of Zinc, Aluminum, Stannum, etc.
CMC-M3-2
Repair high speed steel
Mending cut die & shears
(Design for joining a broad range of high speed steel
High hardness: HRC 61~63, Good machining property
Excellent welding usability)
For welding & stretching, hot work and high hardness tool mold, hot forging general die, hot punch die, screw die, grinding-resisted hard surface, High-speed steel.
CMC-MS-3
Repair Maraging stainless steel
Mending Aluminum gravity casting dies
(Design for repair Maraging stainless steel
Untreated:HRC30-32 After age hardening 2H/500℃:HRC48-52)
Special hardening good toughness alloy, especially adapt to Aluminum gravity cast, gate, be able to extend product's life-span for 3-5 times afterwards. Be able to manufacture the greatly exact mold, super satin process, heat-resisted and crack-resisted when doing gating-weld.
CmC-12Cr
Specially used for Cr12¡BCr12MoV series mold argon welding wire. If more than three layers need to be welded, CMC-30N can be used as the base.
When being used for Cr12 after heat treatment, no need of preheating for small area. The weld hardness is enough, it can be used for mechanical processing.
CMC-Magic1
Very not easy to crack, suitable for high carbon content heat-treated steel.
Be used for embossing & drawing die, which can greatly reduce the scratches caused by bending and stretching between high tension steel and ordinary one.