Specification:
Base Material: Ti(Gr1,Gr2),TA1,TA2
Density of Current: < 3000 A/㎡
Cotent of the florin irons: < 500 mg/L
Coating of material: RuO2+X
Noble metal content: 8-25 g/㎡
Content of hydrochloric acid: < 20 %
Temperature: < 60 ℃
PH value: 1-12
Standards: GB/N ASTM
Properties: application-specific design, tight adhesion between platinum layer and base titanium material, stable performance, light weight ( the lowest weight in all shape of anode ), recoating possible, long service life
Base Material: Ti(Gr1,Gr2),TA1,TA2
Density of Current: < 3000 A/㎡
Cotent of the florin irons: < 500 mg/L
Coating of material: RuO2+X
Noble metal content: 8-25 g/㎡
Content of hydrochloric acid: < 20 %
Temperature: < 60 ℃
PH value: 1-12
Standards: GB/N ASTM
Properties: application-specific design, tight adhesion between platinum layer and base titanium material, stable performance, light weight ( the lowest weight in all shape of anode ), recoating possible, long service life