Conveyor pulley lagging Products range:
ZE-TC Ceramic Lagging :
1.Aluminum Oxide:92%.
2.Ceramic Hardness(Mohs):>9t
3.Working temperature:≤85°C
4.Rubber Hardness: 60±5 Shore A
5.Tensile strength:150Kg/m2
6.With CN bonding
ZE-LZ Pulley Lagging:
1.Technical parameter
1.1.material: synthetic rubber,mainly of BR,IR and SBR.
1.2.Hardness of rubber:
Hardness of non flame-retardant rubber Shore 70±5
Hardness of flame-retardant rubber Shore 70±5
1.3.Abrasion loss:<160mm³
1.4.Thickness of rubber sheet: 8mm,10 mm,12 mm,15 mm,20mm
1.5. Surface of rubber:plain, diamond grooved, strip.
1.6.Dimensions of diomand profile:5*5*20mm
2.We can make products upon your drawings and parameters, and so on .
ZE-WK1 Pulley lagging:
1. Consist of tile shell rubber layer , aluminium layer ; and the tile shell rubber layer was vulcanized to metal layer and slab rubber .
2. Thickness (3 standard types):12mm, 15mm , 20mm.
3. Apply to all sizes of pulley.
ZE-WK2 pulley lagging:
1. To connect the tile shell rubber and bolt , to vulcanize the wear-resistant slab rubber layer and metal layer.
2.thickness:18mm.
3.apply to the demension of pulley which less than Φ1400*1400mm.
4.to settle on site , don't need to tear down.