1 Introduce :As-cast pearlite nodular cast iron nodulizer contains suitable Ca,Ba,Sb and Cu that strengthen effectively the capacity of graphitizing. Therefore the tendency of white is small and the property of anti-aging is good.
2 Specification The Process is simple and the product applies convenience. The additive amount of nodulize is about 1.4-1.8%
Model Number
|
Composition %
|
range of application
|
|||||||
|
Re
|
Mg
|
Si
|
Al
|
Ti
|
Other
|
|
|
|
Pearlite
1
|
Z-1
|
1.0-3.0
|
5.0-7.0
|
38-44
|
≤1.0
|
≤
0.5
|
CaBa SbCuFe
|
Used in electric furnace iron liquid
|
|
Pearlite
2
|
Z-2
|
1.5-3.5
|
7.0-9.0
|
38-44
|
≤1.0
|
≤
0.5
|
CaBa SbCuFe
|
Used in Cannon Iron liquid
|
3 Model Number Z-1,treating temperature is about 1440-1500℃
Model Number Z-2, treating temperature is about 1390-1460℃