Product Main

Specifications

Iron-based amorphous ribbon: Production speciation: Thickness 0.02mm to 0.03mm,width 2.5mm to 170 mm. Customized size is also available upon requests. Physical properties:  Saturate Induction  1.56T             Hardness(Hv)              960kg/mm2        Curie Temperature  410 degress C  Density  7.18g/cm3   Crystallization Temperature      535 degress C  Resistivity  130-cm  Saturate Magnetostriction  2710-6       Magnetic properties:    Product type Transverse field annealed  No field annealed   Longitudinal field annealed  Maximum permeability   >2104   >20104  >25104  Saturate induction  1.5T  1.5T  1.5T  Remanence  <0.5T  01.0T  1.2T  Coercivity  <4 A/m  <2.4 A/m  <4 A/m  Core loss (50kHz, 1.4T)             <0.2 W/kg  <0.13 W/kg  <0.3 W/kg  Core loss (400kHz, 1.2T)  <1.8 W/kg  <1.25 W/kg  <2 W/kg  Core loss (8kHz, 1.0T)  <80 W/kg  <60 W/kg  <100 W/KG   Curves: