Product Main

Specifications

The Performance Advantage of AAC block

 

Lightweight: Porosity achieve 70% to 85%, volume density is generally 500 ~ 900kg/m3, as 1/5 of general concrete the 1/4of clay, the 1/3 of hollow brick, and similar with wood can float in water. It can reduce building weight, reduction in the cost of integrated building.

 

Fireproof: Most of the major raw materials is inorganic materials, so it has good fire resistance, and do not emit harmful gases when meet fire. Fire 650 degrees, as a refractory material, the thick up of 90mm walls can reach to 245 minutes fire resistance, 300mm thick up wall can reach to 520 minutes fire resistance.

 

Sound insulation: Due to a unique porous structure, so it has a sound absorption capacity. The sound absorption capacity can reach of 10mm thick wall up to 41 db.

 

Insulation: As the material inside has a large numbers of the pores and porous, which has a good thermal insulation properties. The Thermal conductivity is 0.11-0.16W/MK, as 1/4-1/5 of brick. Typically, the insulation effect of 20cm thick aerated concrete wall is equivalent to 49cm thick solid brick walls ordinary.

 

Permeability: Result of material by the composition of many independent small pores, the moisture absorption is slow, in the volume of absorbent is 5 times of clay saturation do. When used in the bathroom, the wall can be treated to interface directly paste tiles.

 

Anti-seismic: The same building structure, improve the two seismic than the brick level.

Pro-environment: Manufacturing, transportation, all use the process of pollution, to protect arable land, saving energy, is one kind of a green building material.

 

Durability: material strength is stability, in the specimens tested after one year of atmospheric exposure; the intensity increased by 25%, and remained stable after ten years.

Shortcut: it has good machinability, can be sawed, planed, drilled, nailed, and available appropriate as bonding of adhesive material, so create favorable conditions for building construction.

 

Cost-saving: An integrated lower cost than using more than 5% of solid clay bricks, and can increase the usable area, greatly enhance the utilization of floor space.

 

Main Steps for Produce AAC brick:

1. First, dose and match measured raw materials

2. After distributing, feed raw material into pouring mixer to make slurry

3. Through thoroughly mixing, the slurry is poured to mould

4. After pre-curing under a certain temperature and time, the block would reach certain hardness prepare for cutting

5. Tilting hoister would turn over 90 degree of mould

6. Then open the mould and separate it from block, and take the block with side plate ti cutting cart

7. The blocks then be cut through the cutter firstly of two vertical sides of block

8. Secondly the horizontal cutting

9.  Finally the vertical cutting

10. After cutting, the block is hanged to trolley with side plate by semi-finished product hoister

11. Organizing the cut blocks and put them into autoclave

12. Hardening the blocks under certain temperature and pressure

13. Take finished products out of autoclave

14. The finished product hoister takes the finished product to stock shield

15. Packed for loading

16. The side plate return back by side plate roller

17. Side plate would be organized with open mould

18. Clean the mould and preparing for next pouring

19. Steel bars processing line for slab production