Type: Diameter75-600mm
Name: lmpregated
Description: lmpregated Graphite Electrode
Technical properties of graphite electrode |
1. Physical and chemical index |
ltem |
unit |
Nominal Diameter(mm) |
YB/T4088-2000 |
Typical Values |
Industry Standard |
75-225 |
250-350 |
400-550 |
75-130 |
150-225 |
250-300 |
300-550 |
Electric Resistivity |
Electrode |
μΩ·m |
≤9.0 |
≤9.0 |
≤9.0 |
≤7.5 |
≤7.5 |
≤8.0 |
≤8.5 |
Nipple |
≤7.5 |
≤7.5 |
≤7.5 |
≤6.5 |
≤6.5 |
≤7.0 |
≤7.0 |
Bending strength |
Electrode |
Mpa |
≥10.0 |
≥9.0 |
≥8.0 |
≥10.0 |
≥10.0 |
≥9.0 |
≥8.5 |
Nipple |
≥13.0 |
≥13.0 |
≥13.0 |
≥13.0 |
≥13.0 |
≥13.0 |
≥14.0 |
Elastic modulus |
Electrode |
Gpa |
≤12.0 |
≤12.0 |
≤12.0 |
≤9.3 |
≤9.3 |
≤12.0 |
≤12.0 |
Nipple |
≤14.0 |
≤14.0 |
≤14.0 |
≤14.0 |
≤14.0 |
≤14.0 |
≤14.0 |
Bulk density |
Electrode |
g/cm3 |
≥1.58 |
≥1.58 |
≥1.58 |
≥1.70 |
≥1.69 |
≥1.65 |
≤1.62 |
Nipple |
≥1.68 |
≥1.68 |
≥1.68 |
≥1.72 |
≥1.72 |
≥1.72 |
≤1.72 |
Ash |
Electrode |
% |
≤0.3 |
|
≤0.3 |
≤0.3 |
≤0.3 |
≤0.3 |
≤0.3 |
≤0.3 |
Nipple |
CTE (100-600)℃ |
Electrode |
10-6/℃ |
≤2.7 |
≤2.7 |
≤2.7 |
≤2.6 |
≤2.6 |
≤2.7 |
≤2.7 |
Nipple |
≤2.5 |
≤2.5 |
≤2.5 |
≤2.4 |
≤2.4 |
≤2.5 |
≤2.5 |
|
Current Carrying Capacity And Current Density |
Nominal |
lmpregnated electrode |
diameter |
mm |
inch |
Current load A |
Current density A/cm2 |
75 |
3 |
1300-2000 |
29-45 |
100 |
4 |
1800-3000 |
22-37 |
130 |
5 |
2800-4200 |
21-31 |
150 |
6 |
4000-5000 |
22-28 |
175 |
7 |
3900-6800 |
16-28 |
200 |
8 |
4800-9000 |
15-28 |
225 |
9 |
6400-9700 |
16-24 |
250 |
10 |
8000-12000 |
16-24 |
300 |
12 |
11000-16000 |
15-22 |
350 |
14 |
15000-22000 |
15-22 |
400 |
16 |
18000-23500 |
15-22 |
450 |
18 |
20000-28000 |
15-21 |
500 |
20 |
24000-34000 |
13-20 |
|
|