Type: Diameter300-600mm
Name: High Power
Description: High Power Garphite Electrode
Name: High Power
Description: High Power Garphite Electrode
Technical properties of HP garphite electrode | |||||||
1. Physical and chemical index | |||||||
ltem | unit | Nominal Diameter(mm) | |||||
YB/T4090-2000 | Typical Values | ||||||
Industry Standard | |||||||
200-400 | 450-550 | 300-400 | 450-550 | ||||
Electric Resistivity | Electrode | μΩ·m | ≤7 | ≤7.5 | 5.0-6.6 | 5.4-6.8 | |
Nipple | ≤6.5 | ≤6.5 | 4.0-5.0 | 4.0-5.0 | |||
Bending strength | Electrode | Mpa | ≥10.5 | ≥9.8 | ≥11.0 | ≥11.0 | |
Nipple | ≥14.0 | ≥14.0 | ≥16.0 | ≥16.0 | |||
Elastic modulus | Electrode | Gpa | ≤12.0 | ≤12.0 | ≤11.0 | ≤11.0 | |
Nipple | ≤16.0 | ≤16.0 | ≤15.0 | ≤15.0 | |||
Bulk density | Electrode | g/cm3 | ≥1.60 | ≥1.60 | 1.63-1.70 | 1.63-1.70 | |
Nipple | ≥1.70 | ≥1.70 | 1.73-1.80 | 1.73-1.80 | |||
Ash | Electrode | % | ≤0.3 | ≤0.3 | ≤0.3 | ≤0.3 | |
Nipple | |||||||
CET 100-600℃
|
Electrode | 10-6/℃ | ≤2.4 | ≤2.4 | 1.8-2.2 | 1.8-2.2 | |
Nipple | ≤2.2 | ≤2.2 | 1.5-1.8 | 1.5-1.8 | |||
. Recommended current carrying capacity | |||||||
YB/T4089-2000 | BSTS-HP | ||||||
Nominal Diameter | Current Carrying Capacity | Current Density | Electrical arc furnace | ladle Refining furnace | |||
Current Carrying Capacity | Current Density | Current Carrying Capacity | Current Density | ||||
in | mm | A | A/cm2 | A | A/cm2 | A | A/cm2 |
12 | 300 | 13000-17400 | 17-24 | 13000-17500 | 18-25 | 15000-21000 | 21-29 |
14 | 350 | 17400-24000 | 17-24 | 17500-24500 | 18-25 | 20000-28000 | 21-29 |
16 | 400 | 21000-31000 | 16-24 | 21500-32000 | 17-25 | 24000-35000 | 19-28 |
18 | 450 | 25000-40000 | 15-24 | 26000-40500 | 16-25 | 29000-45000 | 18-28 |
20 | 500 | 30000-48000 | 15-24 | 32000-50000 | 16-25 | 34000-54000 | 17-27 |
22 | 550 | 35000-55000 | 14-22 | 37000-57000 | 15-23 | 40000-62000 | 16-25 |