1.The product is made of multilayer polymer fiber saturated by Polyurethane and polyester.Before use,it needs to be activated by water.The polymer fiber is in non-woven protective layer,which makes patient feel comfortable in use.
2.New material of orthopaedics external fixation!New products substituting plaster padding.
1.EASY-OPERATED DEVICE
The whole operation is finished within 3~5 minutes without any heating equipments but by only using the normal-temperatured water,which not only eases the labour for doctors,but also saves the time of operation.
2.X-RAY PERMISSIBILITY
The doctors can examine the broken parts clearly without removing the casting and splint,which ensure the accuracy and integrity of the operation.
3.EXCELLENT AIR-PERMEABILITY
The holes on the products make good air-pereability and prevent skin from infection,itch and smell.
4.HIGH STRENGTH
The strength are five times that of the plaster products,which can make the injured part protection more effectively.
5.LIGHTWEIGHT
Heshun Cast and Heshun Splint are only 1/5 heavier and 1/3 thicker than plaster products,which makes the pacients feel more comfortable.
6.VARIOUS SPECIFICATION
The products will satisfy different needs of injured parts and color-preference for diff erent ages.
7.ENVIRONMENTAL PROTECTION
Heshun Cast and Heshun Splint are made from polyester or glass fiber.After operation,they can be burnt without pollution.
2.Open the package and take out the splint.Saturate it in water for 3-4 seconds and press it 2-3 times.
3.Take it out and press out the water.Absorb the water with a towel.
4.Plase it on the needed part and fix it with bandage.
5.It will be hardened after 3-5 minutes and be capable of use after 20 minutes.
2.The whole operation must be finished in 3-5 minutes,some delay will affect the shaping effect.Within 10 minutes hardening time, the affected part cannot move.
1.The hardening of the splint has direct relation to the water temperature,temperature is high,hardening quickly,temperature is low,hardening slowly.
5.It will be hardened after 3-5 minutes and be capable of use after 20 minutes.
2.The whole operation must be finished in 3-5 minutes,some delay will affect the shaping effect.Within 10 minutes hardening time, the affected part cannot move.
1.Choose proper specification according to need.
Heshun Cast and Heshun Splint are made from polyester or glass fiber.After operation,they can be burnt without pollution.
2.Open the package and take out the splint.Saturate it in water for 3-4 seconds and press it 2-3 times.
3.Take it out and press out the water.Absorb the water with a towel.
4.Plase it on the needed part and fix it with bandage.
5.It will be hardened after 3-5 minutes and be capable of use after 20 minutes.
2.The whole operation must be finished in 3-5 minutes,some delay will affect the shaping effect.Within 10 minutes hardening time, the affected part cannot move.
1.The hardening of the splint has direct relation to the water temperature,temperature is high,hardening quickly,temperature is low,hardening slowly.
5.It will be hardened after 3-5 minutes and be capable of use after 20 minutes.
2.The whole operation must be finished in 3-5 minutes,some delay will affect the shaping effect.Within 10 minutes hardening time, the affected part cannot move.