Performance Characteristics:
It is a typical high-heat and high-strength mould steel. The main alloying element W content up to 8% or more,this kind of steel has high hardness and high strength after heat treatment.
Applications:
1.High ability of anti-tempering ,it is used to make high stress but no shock loading male mold and female mold.
2.Bending stressor tensile stress mould such as anti-extruding die.
3.Cuttting tool in high temperature stress.
Chemical Composition (%):
C
|
Si
|
Mn
|
Cr
|
W
|
V
|
P
|
S
|
0.30-0.40
|
≤0.40
|
≤0.40
|
2.20-2.70
|
7.50-9.00
|
0.20-0.50
|
≤0.030
|
≤0.030
|
Procedure:
Steps
|
Description
|
Arrange Ingredients
|
Standard or according to customer request
|
Smelt
|
IF furnace
|
Forge
|
Electrical-hydraulic hammer
|
Anneal
|
Annealing furnace
|
Crack Detection
|
UT report
|
Peeled/Turned/Machined
|
As customer requested
|
Adjust
|
To make the dimension more precise
|
Package
|
Suitable for transport
|
Delivery Condition:
Annealed