JM28 JM28
Al2O3 % ≥ 60 67
Fe2O3 % ≤ 0.7 0.6
Bulk Density g/cm3≤ 1.0 1.2
Cold Compress Strength Mpa≥ 4.0 5.0
Thermal Resistance times(1100℃,air cooling) 20 20
Heating Linear Change %(1500℃*12h) ≤ 1 1
Thermal Conductivity W/M.K(350±25℃) ≤ 0.35 0.4
1.has passed ISO
2.can resist high temperature
3.high strength and low thermal conductivity
4.well energy conservation
High Temperature Mullite Insulating Brick,Thermal Insulating Brick,Mullite Brick:
The products are according to the international standard to be manufactured.The mullite brick has low Fe2O3 content,good thermal shock resistance and low thermal conductivity.
The products are according to the international standard to be manufactured.The mullite brick has low Fe2O3 content,good thermal shock resistance and low thermal conductivity.
Application:
Mullite insulating brick is widely used for furnace lining,roller kiln,craking furnace and shuttle kiln,etc.
Technical Data:
Items | JM23 | JM23 | JM26 | JM26 | |
Classification temperature,°C | 1260 | 1350 | 1410 | 1410 | |
Bulk density,g/cm3 ≤ | 0.55~0.6 | 0.8±0.05 | 0.8±0.05 | 1.0±0.05 | |
Cold compressive strength,Mpa | 1.2 | 2.5 | 2.5 | 3.0 | |
Hot load strength(%) deformation | 0.034Mpa |
1100°c
≤0.1
|
|||
Hot load strength(%) deformation | 0.07Mpa |
1100°c
≤0.9
|
1200°c
≤0.2
|
1260°c
≤0.2
|
1260°c
≤0.2
|
Heating linear change,% after 24h | ≤0.5 | ≤0.5 | ≤0.4 | ≤0.5 | |
Al2O3,% ≥ | 40~45 | 54~56 | 55~57 | 55~57 | |
SiO2,% | 47~45 | 39~38 | 38~36 | 38~36 | |
Fe2O3,% ≤ | 0.7~1.0 | 0.7~1.0 | 0.7~1.0 | 0.7~1.0 | |
Thermal conductivity W/m.k @600°c | 0.16 | ||||
Thermal conductivity W/m.k @800°c | 0.18 | 0.31 | 0.31 | 0.35 | |
Thermal conductivity W/m.k @1000°c | 0.20 | 0.33 | 0.33 | 0.37 | |
Thermal conductivity W/m.k @1200°c | 0.35 | 0.35 | 0.41 | ||
Reversible thermal expansion,% @1100°c | 0.5 | ≤0.7 | ≤0.7 | ≤0.8 |
JM28 JM28
Al2O3 % ≥ 60 67
Fe2O3 % ≤ 0.7 0.6
Bulk Density g/cm3≤ 1.0 1.2
Cold Compress Strength Mpa≥ 4.0 5.0
Thermal Resistance times(1100℃,air cooling) 20 20
Heating Linear Change %(1500℃*12h) ≤ 1 1
Thermal Conductivity W/M.K(350±25℃) ≤ 0.35 0.4