Technical
Data
|
Coating Color | Intense Blue |
Thickness | 0.15,0.20,0.25,0.30,0.40mm | |
Sensitive
Wavelength
|
800-850nm | |
Photosensitivity | 50-55mw/1000RPM | |
Dot reproduction | 1%-99% at 240 lpi (2400dpi) | |
Laser Energy | 130-150mj/cm2 (mJ/cmvaries based on plate setter manufacturer)2 | |
Run Length | 120,000-150,000 impressions unbaked.500,000-1,000,000 impressions after post baking.(Actual run length may vary according to press, ink and paper condition.) | |
Plate
Developing
Condition
|
Recommend
Developer
|
HUACAI developer or Kodak or Agfa developer (Fuji Developer is not suitable) |
Developing
Temperature
|
23+/-2 degree Celsius | |
Developing Time | 20-25s | |
Detailed
Information
|
Post Baking
Conditions
|
Apply baking gum before baking
Static Oven:220-230 °C for a duration of 5-8 minutes
(Actual oven settings may vary accoring to oven conditions.)
|
Platesetter
Compatibility
|
Kodak Trendsetter, Kodak Lotem, Kodak Magnus, Screen PT-R, Heidelberg ,Topsetter, Suprasetter and Luscher Xpose! | |
Safe Light | Odinary indoor white light | |
Shelf Life | 18 months under recommended storage conditions (Unopened plate packs should be stored flat and away from excessive cold ,heat and humidity≤65%, temperature≤30°C, stacking height less than 1.5 meters) |