wet strength | >0.3 kg/cm2 | |||
wet-heat tensile strength | ≥16 gf/m2 | |||
glue value | ≥60% | |||
attracts blue quantity | 38g/100g | |||
granularity | 95 | |||
inflation multiple | ≥10 | |||
water content | ≤12% | |||
monmorillonite | >65% | |||
wet-heat tensile strength | 45-55 gf/m2 | |||
glue value | 55-90% | |||
attracts blue quantity | 29 | |||
SiO2 | 65-75 | |||
AiO3 | 13-14 | |||
Fe2O | 1-1.5 | |||
P2O3 | 0.01 | |||
CaO | 2-2.5 | |||
MgO | 2.5-3 | |||
K2O | 0.1-0.5 | |||
Se | 1.2 | |||
Cu | 1.5 | |||
Zn | 32 | |||
Co | 16 | |||
Mo | 0.4 | |||
packing: | 50kg/25kg plastic weave bag | |||
Application: | used in sand casting,asbestos insulation materials and feed additive |