Specifications
Fused cast AZS,castable AZS refractory blocks TY 33#,TY36#,TY 41# for bottle glass/ glaze /frit furnace side wall.
Physical and chemical index
Item
|
Behaviors
|
|||
AZS-33#
ER 1681
|
AZS-36#
ER 1685
|
AZS-41#
ER 1711
|
||
Chemical
Composition
|
Al2O3
|
≥50.00
|
≥49.00
|
≥45.00
|
ZrO2
|
≥32.50
|
≥35.50
|
≥40.50
|
|
SiO2
|
≤15.50
|
≤13.50
|
≤13.00
|
|
Na2O+K2O
|
≤1.30
|
≤1.35
|
≤1.30
|
|
Bulk density g/cm3
|
≥3.75
|
≥3.85
|
≥4.00
|
|
Apparent Porosity %
|
≤1.2
|
≤1.0
|
≤1.2
|
|
Cold Crushing Strength Mpa
|
≥300
|
≥300
|
≥300
|
|
Exudation Temperature of Glass Phase
|
≥1400
|
≥1400
|
≥1410
|
|
Bubble Separation Ratio(1300°C×10h)
|
≤1.2
|
≤1.0
|
≤1.0
|
|
Anti-corrosion rate of glass liquid
1500°C×36h (mm/24h)%
|
≤1.4
|
≤1.3
|
≤1.2
|
|
Apparent density
(g/cm3)
|
PT(RN RC N)
|
≥3.50
|
≥3.50
|
≥3.70
|
ZWS(RR EVF EC ENC)
|
≥3.65
|
≥3.70
|
≥3.90
|
|
WS( RT VF EPIC FVP DCL)
|
≥3.75
|
≥3.8
|
≥4.00
|