This product can make water reducer much higher W/B ratio
shrinkage and creep
low-alkali
low foaming
low consumption
Product application
1. Under the same intensity of the slump, joining the DongKe water reducer can save cement of 25-30%.
2. To the hardening accelerating agent and reinforce have obvious effect. Concrete mixed with HSB, for 3 days to reach the design strength of 60-70%,for 7 days to reach 100%,for 28 days to cincreased 30-40% compared with the blank concrete strength.