Product Main

Specifications

the product features
The junction surface’s roughness( RA)should not be lowering 3.2  in the  structure of gypsum block forming mould.
the roughness(Ra) of working surface among the forming machine mould , the evacuating pipe and the material contact surface should not be lowering 1.6,our company has achieved 1.6-0.8 and has exceeded the national standard.
We choose hard chromium plating  as the aseptic technic,which is not easy to rust and helps lengthening  the service life. 
We choose leakproof structure so as to keep not leaking the liquid and avoid producing hard friction with the working surface,and lengthen the service life as well.