STEEL BALL PRECISION GRADE
GRADE |
VDWS BALL DIAMETER |
SPH DEVIATION FROM |
VDWL LOT DIAMETER |
RA MAXIMUM |
G5 |
0.13 |
0.13 |
0.25 |
0.014 |
G10 |
0.25 |
0.25 |
0.5 |
0.020 |
G16 |
0.4 |
0.4 |
0.8 |
0.025 |
G20 |
0.5 |
0.5 |
1 |
0.032 |
G24 |
0.6 |
0.6 |
1.2 |
0.040 |
G28 |
0.7 |
0.7 |
1.4 |
0.050 |
G40 |
1 |
1 |
2 |
0.060 |
G60 |
1.5 |
1.5 |
3 |
0.080 |
G100 |
2.5 |
2.5 |
5 |
0.100 |
G200 |
5 |
5 |
10 |
0.150 |
G500 |
12.5 |
12.5 |
25 |
|
G1000 |
25 |
25 |
50 |
|
STAINLESS STEEL CHEMICAL COMPOSITION
MATERIAL CODE |
CHEMICAL COMPOSITION(%) |
||||||||
AISI |
C |
Si |
Mn |
P |
S |
Cr |
Ni |
Mo |
other |
302 |
≤0.15 |
≤1.00 |
≤2.00 |
≤0.045 |
≤0.030 |
17.00-19.00 |
8.00-10.00 |
__ |
__ |
304 |
≤0.08 |
≤1.00 |
≤2.00 |
≤0.045 |
≤0.030 |
18.00-20.00 |
8.00-10.50 |
__ |
__ |
316L |
≤0.030 |
≤1.00 |
≤2.00 |
≤0.045 |
≤0.030 |
16.00-18.00 |
10.00-14.00 |
20.00-3.00 |
__ |
420 |
≤0.15 |
≤1.00 |
≤1.00 |
≤0.040 |
≤0.030 |
12.00-14.00 |
__ |
__ |
__ |
430 |
≤0.12 |
≤1.00 |
≤1.00 |
≤0.040 |
≤0.030 |
16.00-18.00 |
__ |
__ |
__ |
440C |
0.95-1.20 |
≤1.00 |
≤1.00 |
≤0.040 |
≤0.030 |
16.00-18.00 |
__ |
≤0.75 |
__ |
STEEL BALL CONVERSION TABLE
|
|