1. Grade: Y10T,Y20,Y25,Y30,Y30BH,Y35(China standard);C1,C5,C8,C11(U.S.A. Standard) HF8/22- HF24/3(Europe standard)
2. Shape: Arc, Block, Bar, Ring, Cube, Disc, or others
3.Size: D76*40*8 mm
4. Quality 1st
Ferrite magnets are composed of barium or strontium ferrite and manufactured with ceramic
processing technology. They are very hard and brittle which requires professional and
specialized machining techniques. Popular for a wide range of low cost applications.
1.Inexpensive at medium to low magnetic strength.
2.Can be magnetized with multiple poles on one or both pole surfaces.
3.High coercive force.
4.Working temperature is up to 450 degree
5.Good resistance to demagnetization.
6.Does not rust, no surface treatment required.
Density:4.6~5.0g/cm3
Saturation magnetizing field required: about 10KOe
Manufacture method: dry press and wet press. The dry process is used for isotropic and
anisotropic material, and the wet method applies only to the production of anisotropic
material.
Shape available: blocks, bars, discs, rings, arc segments, etc.
Grade available: C1 to C11, Br from 230MT to 430MT
Advantages:
1. We have been in this field of business over 10 years, in which time we have gained much valuable manufacturing experience and full-range facilities as well as advanced technology.
2. We are a magnetic material company with integration of processing and marketing, which guarantees high quality, competitive prices and all-round services.
2. Shape: Arc, Block, Bar, Ring, Cube, Disc, or others
3.Size: D76*40*8 mm
4. Quality 1st
Ferrite magnets are composed of barium or strontium ferrite and manufactured with ceramic
processing technology. They are very hard and brittle which requires professional and
specialized machining techniques. Popular for a wide range of low cost applications.
1.Inexpensive at medium to low magnetic strength.
2.Can be magnetized with multiple poles on one or both pole surfaces.
3.High coercive force.
4.Working temperature is up to 450 degree
5.Good resistance to demagnetization.
6.Does not rust, no surface treatment required.
Density:4.6~5.0g/cm3
Saturation magnetizing field required: about 10KOe
Manufacture method: dry press and wet press. The dry process is used for isotropic and
anisotropic material, and the wet method applies only to the production of anisotropic
material.
Shape available: blocks, bars, discs, rings, arc segments, etc.
Grade available: C1 to C11, Br from 230MT to 430MT
Advantages:
1. We have been in this field of business over 10 years, in which time we have gained much valuable manufacturing experience and full-range facilities as well as advanced technology.