Silicone Rubber Glassfiber sleeving(inside glassfiber and outside silicone rubber)
Details:
Silicone Rubber Glassfiber insulating Sleeving(inside glassfiber and outside silicone rubber) is braided into tubes with non-alkali glassfiber, and then painted with silicone rubber through high temperature. It has better features than silicone glassfiber tubes in the aspect of electricity-avoidness, flame off-self and flexibility. It is widely used in insulating protection of H & N Grade automobile, shipbuiding,electrical machinery, home appliance, electric & heat equipment, special lightware. etc
Inside diameter measurement
|
|
|
|
Inside diameter
|
Wall thickness
|
||
Range
|
Tolerance
|
4000V
|
7000V
|
0.5-2.0mm
|
+0.20-0.00mm
|
0.40±0.05mm
|
0.45±0.05mm
|
2.5-3.0mm
|
+0.25-0.00mm
|
0.40±0.05mm
|
0.50±0.05mm
|
3.5-5.0mm
|
+0.35-0.00mm
|
0.50±0.05mm
|
0.50±0.05mm
|
6.0-9.0mm
|
+0.50-0.00mm
|
0.55±0.05mm
|
0.60±0.05mm
|
10.0-12.0mm
|
+0.70-0.00mm
|
0.60±0.05mm
|
0.65±0.05mm
|
13.0-20.0mm
|
+0.80-0.00mm
|
0.65±0.05mm
|
0.70±0.05mm
|
22.0-35.0mm
|
+0.90-0.00mm
|
1.00±0.05mm
|
1.05±0.05mm
|
|
|
|
|
Specification:
|
|
|
|
ITEM
|
VALUE
|
||
Continuous Operating Temperature
|
-10oC+200oC
|
||
Temperature Endurance
|
265oC±2oC168>1/2 Original value of voltage
|
||
Aging Test
|
260oC,6 hrs without crackle
|
||
Cold bend
|
Witout crackle
|
||
Horizontal Flame Test
|
<30 seconds
|
||
(V W-1)Flame Retardance
|
<30 seconds
|
||
Submerge Water Test
|
Not-sticky,non-deformed,non bated
|
||
Temperature-resistunce
|
+200oC-10oC
|
||
Average-voltage
|
4000V-7000V
|
||
Individual Value
|
2500V-5000V
|