(sdhhcasting.com/wear-resisting-pipe/4253699.html)
Material:KmTBCr5MoG,KmTBCr15MoG,KmTBCr26NiMoG
Process: Lost Foam Process
Wall thickness:10--20mm
Pipe size:≧DN60
main machinery, mechanical, using performance of Bimetal composite wear-resistant pipe.
1.Bimetal composite wear-resistant pipe: working temperature 600 ℃ or less;
2.Metal thermal expansion coefficient of Wear-resisting layer : (11.65~13.75)×106 (mm/mm·℃),and this is very close to outer metal thermal expansion coefficient. The closer of the thermal expansion coefficient means the closer speed of heat expansion and thermal contraction.