Standard: | AISI,ASTM,BS,DIN,GB,JIS |
---|---|
Grade: | 1000 Series |
Thickness: | 6.0mm |
Place of Origin: | China (Mainland) |
Brand Name: | Kun Liu Sheng |
Model Number: | |
Type: | Steel Plate |
Technique: | Hot Rolled |
Surface Treatment: | Coated |
Application: | cooking pan,cooking pot,kitchen utensil |
Special Use: | High-strength Steel Plate |
Width: | |
Length: |
Quick Details
Specifications
1.Double layers composite pot billet
*stainless steel 304 + Aluminum1050
*zDiameter ≤550mm,thickness≤6.0mm
regular thickness :1.5mm,2.0mm,2.5mm,3.0mm
2.Three layers composite pot billet
*stainless steel 304+Carbon steel +stainless steel 304/SS 430
*stainless steel 304+Aluminum1050+stainless steel 304/SS 430
*stainless steel 304+Aluminum1050+copper T2
*Diameter≤550mm,
regular thickness:2.0mm,2.5mm,3.0mm,3.5mm
*Thickness of top layer stainless steel≥0.4mm,bottom layer thickness≥0.6mm
3.Five layers composite pot billet
*SS304+Aluminum 1050+Copper T2+Aluminum 1050+SS 304/SS 430
*SS304+Aluminum1050+Aluminum3003+Aluminum1050+SS 304/SS 430
*Diameter ≤550mm, regular thickness range:2.5mm,3.0mm,3.5mm,4.0mm
*Thickness of top layer stainless steel≥0.4mm,bottom layer thickness≥0.6mm
4.Seven layers composite pot billet
*SS304+Aluminum1050+copperT2+Aluminum1050+copperT2+Aluminum 1050+SS 304/430
*Diameter ≤550mm, regular thickness range:3.0mm,3.5mm,4.0mm,4.5mm
*Thickness of top layer stainless steel≥0.4mm,bottom layer thickness≥0.6mm
Why choosing the stainless steel composite material
*SS304 is a kind of hygienic material and there won't be any polution migrate to the food , ensuring the health cooking and no harm to human body.
*compare with the regular pure stainless steel, with the use of the aluminum,the composite material can enhance the overall heat conductivity and uniform the heat of the pan.
*For five layers &seven layers cladding billet,the inner cladding part (al+cu+al) offer better thermal conductivity and storage the heat, can save the heat energy.
*Aluminum alloy can provide better mechanical property to enhance the overall strength.
*The bottom layer material can be SS304 or SS430,depends on the heating type. SS 304 can not use the electromagnetism heating. For SS 430