ow density polyethylene granules plastic raw materials prices for cable sheath
| No. | Property | Unit | Test | Data |
| 1 | Melt Flow Index | g/10min | GB/T3682-2000 | ≤1.0 |
| 2 | Density | g/cm3 | GB/T1033.1-2008 | ≤0.945 |
| 3 | Tensile strength | Mpa | GB/T1040.3-2006 | ≥14.0 |
| 4 | Elongation at break | % | GB/T1040.3-2006 | ≥600 |
| 5 | Brittle temperature at low temperature | °C | GB/T5470-2008 | ≤-76 |
| 6 | ESCR ,FO | H | GB/T2951.41-2008 | ≥500 |
| 7 | Content of Carbon black | % | GB/T2951.41-2008 | 2.60±0.25 |
| 8 | Carbon Black dispersion | -- | GB/T18251-2000 | ≤3 |
| 9 | Tensile strength after thermal aging | Mpa | GB/T2951.12-2008 | ≥13 |
| 10 | Elongation after thermal aging | % | GB/T2951.12-2008 | ≥500 |
| 11 | Dielectric strength | Mv/m | GB/T1408.1-2006 | ≥25 |
| 12 | Volume resistivity | Ω.m | GB/T1410-2006 | ≥1*1014 |
| 13 | Change rate of tensile strength after weather aging environment of 0--1008h | % | GB/T12527-2008 | ±25 |
| Change rate of elongation after weather aging environment of 0--1008h | % | GB/T12527-2008 | ±25 | |
| Change rate of tensile strength after weather aging environment of 504--1008h | % | GB/T12527-2008 | ±15 | |
| Change rate of elongation after weather aging environment of 504--1008h | % | GB/T12527-2008 | ±15 |