Application: | Welding materials |
---|---|
Diameter: | 2.5mm-5.0mm |
Operating Temperature: | Common |
Welding Current: | DC,AC |
Operating Current: | 40-230A |
Length: | 300-400mm |
Material: | Steel Alloy |
Brand Name: | Jinlongju |
Place of Origin: | China (Mainland) |
Application: | Welding material |
Diameter: | 2.5mm-5.0mm |
Operating temperature: | common |
Welding current: | Dc, AC |
Operating current: | 40-230A |
Length: | 300-400mm |
Material: | Steel alloy |
Quick Details
Specifications
1. Dry the electrodes at 70~100 (158~212 ) for 30~60 minutes before use.
2. Pay attention not to exceed the range of proper currents.
Chemical Composition |
C |
Mn |
Si |
S |
P |
Guarantee Value |
≤0.12 |
0.3-0.6 |
≤0.35 |
≤0.035 |
≤0.040 |
Mechanical Properties of Deposited Metal
Test Item |
Rm(MPa) |
ReL(Mpa) |
A(%) |
KV2(J) |
KV2(J) |
Guarantee Value |
≥420 |
≥330 |
≥17 |
-(normal temperature) |
-(0℃) |
Reference Current (AC, DC)
Electrode Diameter(mm) |
φ2.0 |
φ2.5 |
φ3.2 |
φ4.0 |
φ5.0 |
Length(mm) |
300 |
300(350) |
350 |
400 |
400 |
Welding Current (A) |
40~70 |
55~95 |
80~130 |
120~180 |
160~230 |
V-up, OH |
35~60 |
45~90 |
60~120 |
100~160 |
120~200 |