Application: | High Temperature |
---|---|
Material: | Composite Polymer |
Type: | Insulation Sheet |
Model Number: | XK-P60 |
Brand Name: | GLPOLY |
Place of Origin: | China (Mainland) |
Quick Details
Specifications
unit |
XK-P12 |
XK-P15 |
XK-P25 |
XK-P30 |
XK-P45 |
XK-P50 |
XK-P60 |
XK-P80 |
Method |
||
Reinforcement Carrier |
With (F) or Without Fiber |
Hard Layer (H) or Without Fiber |
|||||||||
Inherent Surface Tack |
2-side |
2-side |
2-side |
2-side |
2-side |
2-side |
2-side |
2-side |
|||
Color |
Gray |
Green |
Yellow |
Light Blue |
Gray |
Red |
Gray |
light Gray |
visual |
||
Thickness |
mm |
0.3~5.0 |
0.3~5.0 |
0.3~5.0 |
0.3~5.0 |
0.3~3.0 |
0.3~3.0 |
0.3~3.0 |
0.5~2.0 |
ASTM D374 |
|
Specific Gravity |
g/cm3 |
2.12 |
2.44 |
2.73 |
3.1 |
3.24 |
3.35 |
3.45 |
3.55 |
ASTM D792 |
|
Hardness |
Asker C |
3~4 |
3~5 |
15~18 |
15~20 |
25~30 |
25~30 |
35~40 |
50 |
JIS K7312 |
|
Shore 00 |
25~35 |
30~40 |
40~50 |
40~50 |
45~55 |
45~55 |
50~60 |
80 |
ASTM D2240 |
||
Thermal impedance @0.5mm 14.5psi |
℃in2/W |
0.65 |
0.59 |
0.35 |
0.28 |
0.26 |
0.21 |
0.16 |
0.13 |
ASTM D5470 |
|
Thermal Conductivity |
W/mK |
1.2 |
1.5 |
2.5 |
3 |
4.5 |
5 |
6 |
8 |
HOT DISK |
|
Volume Resistivity |
Ωcm |
>1013 |
>1013 |
>1013 |
>1013 |
>1013 |
>1013 |
>1013 |
>1013 |
ASTM D257 |
|
Breakdown Voltage |
KV/mm |
15 |
15 |
15 |
15 |
16 |
16 |
16 |
15 |
ASTM D149 |
|
Dielectric Constant |
1 |
5.2 |
5.5 |
6.5 |
7 |
8 |
8 |
8.5 |
9 |
ASTM D150 |
|
Application temperature |
℃ |
-40~160 |
-40~160 |
-50~200 |
-50~200 |
-50~200 |
-50~200 |
-50~200 |
-50~200 |
||
Tensile strength |
psi |
14 |
15 |
13 |
13 |
23 |
12 |
10 |
10 |
ASTM D149 |
|
Elongation |
% |
200 |
130 |
100 |
80 |
50 |
40 |
30 |
20 |
ASTM D149 |
|
Siloxane Volatiles D4~D20 |
% |
<0.01 |
<0.01 |
<0.01 |
<0.01 |
<0.005 |
<0.005 |
<0.003 |
<0.001 |
GC-FID |
|
Flammability |
UL94 |
V-0 |
V-0 |
V-0 |
V-0 |
V-0 |
V-0 |
V-0 |
V-0 |
UL94 |