Product Main

Specifications

Mechanical Properties Comparison:
 Material Tensile Strength MPa Yield Strength MPa Hardness HB Elongation %
Conventional casting 7xxx Al 480-560 430-470  150  8%-9%
Rapid solidification 7xxx Al 600-730 580-670  200 10-12%
Physical Properties Comparison:
7000 Aluminum Alloys Grain Size Segregation Degree Yield Ductility Stress Corrosion Resistance
Conventional casting  80-300μm generate macro segregation 40-50% poor ductility  fair
Rapid solidification  3-25μm no macro segregation 70-80% high ductility 3-5 times of common
7000 aluminum alloys