Section Shape: | Round |
---|---|
Outer Diameter: | 20-1420 mm |
Thickness: | 2.5-60 mm |
Grade: | 10#-45#,15NiCuMoNb5,API J55-API P110,Q195-Q345 |
Grade: | 20#,45#,15NiCuMoNb5,API L80,Q215,Q235,Q345 |
Standard: | API |
Standard: | API 5CT,API 5L |
Outer Diameter: | 20~1420mm |
Alloy Or Not: | Is Alloy |
Special Pipe: | API Pipe |
Surface Treatment: | According to customers' requirements |
Certification: | API |
Technique: | ERW |
Application: | Condenser pipe,heat transfer tube, |
Secondary Or Not: | Non-secondary |
Place of Origin: | China (Mainland) |
Wall thickness(mm) of outer backing pipe: | 2.5~50mm |
Wall thickness(mm) of liner steel pipe: | 0.2~6mm |
Quick Details
Specifications
Nickel matrix, can resistant corrosion in some medium, called the nickel-based corrosion resistant alloy.
the main alloying elements of nickel-based alloys are copper,Chromium and molybdenum. It has a good overall performance, resistance to various acid corrosion and stress corrosion. the first application (1905 US production) is a nickel-copper (Ni-Cu) alloy, also known as Monel (Monel alloy Ni70Cu30). There are also nickel-chromium (Ni-Cr) alloys (nickel-based heat-resistant alloy), nickel-molybdenum (Ni-Mo) alloys (mainly refers Hastelloy B series), nickel chromium-molybdenum (Ni-Cr-Mo) alloys (mainly refers Hastelloy C series) and the like. At the same time, pure nickel is a typical representative of nickel based corrosion resistant alloys. these nickel-based corrosion resistant alloy is mainly used in the manufacture of petroleum, chemical, power and other corrosion-resistant components of the environment.
Application:
L Subsea Pipeline
L Offshore Oil & Gas pipeline
L Onshore Oil & Gas pipeline
L Oil Refining & Petrochemical pipeline
L Power Plant pipeline
L Environmental Protection & Sewage Treatment
Specification:
L Outer Diameter(mm): 20~1420
L Wall thickness(mm):Outer backing pipe 2.5~50;Liner steel pipe 0.25~7
L Composite Standard: API-5LD; DNV-OS-F101; DEP 31.40.20.32; CJ/T192;
L Packing: In bulk or according to customers' requirements
the gripping force(σy) between the lining and the backing steel
Thickness of the lining /mm |
the gripping force(σy) /MPaG |
Remark |
≥3.0 |
≥150 |
|
2.0~3.0 |
≥90 |
|
1.0~2.0 |
≥60 |
|
<1.0 |
- |
Untested |