Brand Name: | Boris Printing Ink |
---|---|
Printing Type: | Screen Printing |
Type: | Solvent Based Ink |
Color: | Pale Gold |
Shelf Life: | 36 months |
Place of Origin: | China (Mainland) |
Quick Details
Specifications
Gloss PVC ink
1. Substrates:
PVC, wood, artificial leather, paper, etc.
2. Applicable products:
PVC inflatable toys, daily necessities, shoes, hats & caps, bags, balls, etc.
3. Product features:
Glossy, strong Coverage, stackable, soft.
4. Test items & test results:
Adhesion: good |
Scratch resistance: 4 |
Wear resistance: 4 |
Migration resistance: 2-3 |
Acid resistance: 3-5 |
Alkali resistance: 3-5 |
Crumpling resistance: 3-5 |
5. Product parameters:
Color shade: refer to Color card |
Color concentration:≥80% |
Fineness:≤7um |
Viscosity: 100-180p |
Gloss: 65-95 |
Liquidity: 20-30mm/s |
Solid content:≥30% |
6. Instructions:
(1) Mesh: 150-300(60-120T) polyester mesh
(2) Squeegee: Polyurethane squeegee at the hardness 65-85 is recommended.
(3) Indicative Dosage: 30/ on the 250(100T) mesh
(4) Drying: natural drying (surface drying in 7-15 mins, Full drying in more than 30 mins) or heat drying at temperature 60℃
(5) Selective Solvents: solvent 007(quick drying, medium Drying, slow drying); fast drier 719, medium drier 718 or slow drier 783 based on printing conditions.
(6) Stencil cleaning: organic solvent (e.g. Mesh washing Agent 007)
7. Notes:
(1) after-tack phenomena will occur while printing on Flexible PVC, which contains plenty of plasticizer. so avoiding stack or isolating with isolating paper is needed for the printing using such kind of ink.
(2) Color migration will occur while printing on Flexible PVC using ink 203, 206, 302, 308 and all fluorescent inks. so good Anti-migration inks are recommended for it, such as ink 2030, 2060, 3020 or 3038.
(3) the anti-penetrability of pigment and substrate will easily lead to color change while printing color matching Ink on flexible PVC. so it is reminded to pay attention to the color feature or amount.
(4) the printing inks with color number 501, 801, 901 or 902 are slightly conductive and will easily produce the spark under High-frequency treatment, so they must be replaced with insulated black 500, Insulated gold 500 or insulated silver 500.
(5) Please pay attention to the solvents Effect on substrate while using 783 or cyclohexanone as the thinner when Printing on flexible PVC.
8. Package:
1, 5, 20kg/barrel
9. Storage:
It can be stored for 36 months at 5-35℃. Keep away from strong light. Avoid strong acid and strong alkali.
10. Warm prompts:
(1) Please thoroughly read the instructions and make a sample test before use.
(2) the technical data is for reference only.
the
END